System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
(Viewing data as-entered.
Click here
to return)
Envalior Pocan® B 1600 000000 PBT
Categories:
Polymer
;
Thermoplastic
;
Polyester, TP
;
Polybutylene Terephthalate (PBT)
;
Polybutylene Terephthalate (PBT), Unreinforced, Molded
Material Notes:
PBT, non-reinforced, injection molding, extrusion, food contact
Former Lanxess product line is now with Envalior.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Bulk Density
0.800
g/cc
ISO 60
Density
1.30
g/cc
ISO 1183
Moisture Absorption at Equilibrium
0.20 %
50% RH; ISO 62
Water Absorption at Saturation
0.50 %
ISO 62
Viscosity Test
140
cm³/g
Viscosity Number; ISO 1628-5
Linear Mold Shrinkage, Flow
0.018
cm/cm
150x105x3; 260 °C / MT 80 °C; 600 bar; ISO 2577
Linear Mold Shrinkage, Transverse
0.018
cm/cm
150x105x3; 260 °C / MT 80 °C; 600 bar; ISO 2577
Melt Flow
570
g/10 min
@Temperature 260 °C
Göttfert, 165 1/s
14
g/10 min
@Load 2.16 kg,
Temperature 260 °C
ISO 1133-1
Mechanical Properties
Original Value
Comments
Puncture Resistance
4275
N
@Temperature -30.0 °C
ISO 6603-2
Ball Indentation Hardness
120
MPa
ISO 2093-1
Tensile Strength, Yield
55.0
MPa
50 mm/min; ISO 527-1,-2
Elongation at Break
>= 50 %
50 mm/min, Nominal; ISO 527-1,-2
Elongation at Yield
4.0 %
50 mm/min; ISO 527-1,-2
Tensile Modulus
2600
MPa
1 mm/min; ISO 527-1,-2
Flexural Strength
85.0
MPa
2 mm/min; ISO 178-A
Flexural Yield Strength
75.0
MPa
@Strain 3.5 %
2 mm/min; ISO 178-A
Flexural Modulus
2650
MPa
2 mm/min; ISO 178-A
Flexural Strain at Break
6.0 %
2 mm/min; ISO 178-A
Izod Impact, Notched (ISO)
<=
10.0
kJ/m²
@Temperature 23.0 °C
ISO 180-1A
<=
10.0
kJ/m²
@Temperature -30.0 °C
ISO 180-1A
<=
10.0
kJ/m²
@Temperature -40.0 °C
ISO 180-1A
Izod Impact, Unnotched (ISO)
160
kJ/m²
@Temperature -30.0 °C
ISO 180-1U
NB
@Temperature 23.0 °C
ISO 180-1U
Charpy Impact Unnotched
200
kJ/m²
@Temperature -30.0 °C
ISO 179-1eU
NB
@Temperature 23.0 °C
ISO 179-1eU
Charpy Impact, Notched
<=
10.0
kJ/m²
@Temperature 23.0 °C
ISO 179 1eA
<=
10.0
kJ/m²
@Temperature -30.0 °C
ISO 179 1eA
Tensile Creep Modulus, 1 hour
2200
MPa
ISO 899-1
Tensile Creep Modulus, 1000 hours
1300
MPa
ISO 899-1
Electrical Properties
Original Value
Comments
Dielectric Constant
3.2
@Frequency 1e+6 Hz
IEC 60250
3.4
@Frequency 100 Hz
IEC 60250
Dielectric Strength
30.0
kV/mm
@Thickness 1.00 mm
IEC 60243-1
Comparative Tracking Index
300
V
Solution A; IEC 60112
425
V
Solution B; IEC 60112
Thermal Properties
Original Value
Comments
CTE, linear, Parallel to Flow
120
µm/m-°C
@Temperature 23.0 - 55.0 °C
ISO 11359-1,-2
CTE, linear, Transverse to Flow
130
µm/m-°C
@Temperature 23.0 - 55.0 °C
ISO 11359-1,-2
Thermal Conductivity
0.250
W/m-K
ISO 8302
Melting Point
225
°C
10°C/min; ISO 11357-1,-3
Maximum Service Temperature, Air
190
°C
IEC 60695-10-2
Deflection Temperature at 0.46 MPa (66 psi)
160
°C
ISO 75-1,-2
Deflection Temperature at 1.8 MPa (264 psi)
60.0
°C
ISO 75-1,-2
Deflection Temperature at 8.0 MPa
45.0
°C
ISO 75-1,-2
Vicat Softening Point
180
°C
@Load 5.10 kg
50°C/h; ISO 306
Flammability, UL94
HB
@Thickness 0.800 mm
HB
@Thickness 1.60 mm
Oxygen Index
24 %
Method A; ISO 4589-2
Glow Wire Flammability Index
750
°C
@Thickness 2.00 mm
IEC 60695-2-12
Shrinkage, MD
0.50 %
@Treatment Temp. 150 °C,
Time 3600 sec
Flow Direction Post-Molding, 150x105x3; ISO 2577
Shrinkage, TD
0.50 %
@Treatment Temp. 150 °C,
Time 3600 sec
Post-Molding, 150x105x3; ISO 2577
Processing Properties
Original Value
Comments
Melt Temperature
260
°C
injection molding; ISO 294
Mold Temperature
80.0
°C
injection molding; ISO 294
Drying Temperature
120
°C
Dry Time
4.00
-
8.00
hour
Moisture Content
0.00 - 0.020 %
Karl Fischer
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
Users viewing this material also viewed the following:
Overview of materials for Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Unreinforced
Evonik Vestodur® HI19 Polymer Modified PBT
Envalior Pocan® B 1505 Z 000000 PBT
Envalior Pocan® B 1100 000000 PBT
DuPont Mobility and Materials Crastin® 6134 NC010 PBT
PLANW9188 / 208393
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.