MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Envalior Durethan® AKV 30 G HR DUS023 900116 Nylon 66 (PA66), 30% Glass Fiber Reinforced, Dry
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 30% Glass Fiber Filled

Material Notes: PA 66, 30% glass fibers, injection molding, improved flowability, hydrolysis stabilized, improved surface finish, GIT/WIT

Former Lanxess product line is now with Envalior.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.343 g/ccISO 1183
Linear Mold Shrinkage, Flow 0.0064 cm/cm60x60x2; 290 °C / MT 80°C; 600 bar; ISO 294-4
Linear Mold Shrinkage, Transverse 0.0082 cm/cm60x60x2; 290 °C / MT 80°C; 600 bar; ISO 294-4
 
Mechanical PropertiesOriginal ValueComments
Puncture Resistance 650 N
@Temperature -30.0 °C
ISO 6603-2
 800 N
@Temperature 23.0 °C
ISO 6603-2
Tensile Strength at Break 135 MPa5 mm/min; ISO 527-1,-2
Elongation at Break 3.2 %5 mm/min; ISO 527-1,-2
Tensile Modulus 8500 MPa1 mm/min; ISO 527-1,-2
Flexural Strength 215 MPa2 mm/min; ISO 178-A
Flexural Yield Strength 210 MPa
@Strain 3.5 %
2 mm/min; ISO 178-A
Flexural Modulus 8000 MPa2 mm/min; ISO 178-A
Flexural Strain at Break 3.8 %2 mm/min; ISO 178-A
Izod Impact, Notched (ISO) <= 10.0 kJ/m²
@Temperature 23.0 °C
ISO 180-1A
 <= 10.0 kJ/m²
@Temperature -30.0 °C
ISO 180-1A
Izod Impact, Unnotched (ISO) 45.0 kJ/m²
@Temperature -30.0 °C
ISO 180-1U
 60.0 kJ/m²
@Temperature 23.0 °C
ISO 180-1U
Charpy Impact Unnotched 55.0 kJ/m²
@Temperature -30.0 °C
ISO 179-1eU
 70.0 kJ/m²
@Temperature 23.0 °C
ISO 179-1eU
Charpy Impact, Notched <= 10.0 kJ/m²
@Temperature 23.0 °C
ISO 179 1eA
 <= 10.0 kJ/m²
@Temperature -30.0 °C
ISO 179 1eA
Puncture Energy 2.00 J
@Temperature -30.0 °C
ISO 6603-2
 2.50 J
@Temperature 23.0 °C
ISO 6603-2
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 30.0 µm/m-°C
@Temperature 23.0 - 55.0 °C
ISO 11359-1,-2
CTE, linear, Transverse to Flow 90.0 µm/m-°C
@Temperature 23.0 - 55.0 °C
ISO 11359-1,-2
Melting Point 259 °C10°C/min; ISO 11357-1,-3
Deflection Temperature at 0.46 MPa (66 psi) 245 °CISO 75-1,-2
Deflection Temperature at 1.8 MPa (264 psi) 200 °CISO 75-1,-2
Deflection Temperature at 8.0 MPa 75.0 °CISO 75-1,-2
Shrinkage, MD 0.050 %
@Treatment Temp. 120 °C,
Time 14400 sec
Flow Direction Post-Molding, 60x60x2; ISO 294-4
Shrinkage, TD 0.040 %
@Treatment Temp. 120 °C,
Time 14400 sec
Post-Molding, 60x60x2; ISO 294-4
 
Processing PropertiesOriginal ValueComments
Melt Temperature 290 °Cinjection molding; ISO 294
 280 - 300 °C
Mold Temperature 80.0 °Cinjection molding; ISO 294
 80.0 - 120 °C
Drying Temperature 80.0 °C
Dry Time 2.00 - 6.00 hour
Moisture Content 0.030 - 0.12 %Karl Fischer

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Grupo Repol Dinalon® A1S25 G30 PA66 30% Glass Fiber
Envalior Durethan® AKV 30 H3.0 000000 Nylon 66 (PA66), 30% Glass Fiber Reinforced, Conditioned
Envalior Durethan® AKV 30 H2.0 901510 Nylon 66 (PA66), 30% Glass Fiber Reinforced, Dry
Envalior Durethan® AKV 30 H2.0 901510 Nylon 66 (PA66), 30% Glass Fiber Reinforced, Conditioned
Envalior Durethan® AKV 30 GIT H2.0 900116 Nylon 66 (PA66), 30% Glass Fiber Reinforced, Dry

PLANW9216 / 208013

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.