Characteristics: Promyde B40 LN is a high viscosity polyamide 6 heat stabilized, lubricated and nucleated for injection molding. Applications: Promyde B40 LN is typically used for the manufacture of small resistant wheels required to support weight such as glass doors, also small technical parts where more resistance to wear and tear is needed over standard viscosity polyamide. Information provided by Nurel Engineering Polymers |