Description: AKROMID B3 GF 35 1 natural is a 35% glass fiber reinforced, heat aging resistant polyamide 6 with high rigidity and strength and light inherent color. Applications are mainly components in mechanical engineering and in the automotive industry. Features: - Good Heat Aging Resistance
- High Stiffness
- High Strength
Uses:- Automotive Application
- Engineering Parts
Information provided by Akro-Plastic GmbH |