System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
(Viewing data as-entered.
Click here
to return)
Southern Polymer PRIMALENE® WPP620Q LLDPE
Categories:
Polymer
;
Thermoplastic
;
Polyethylene (PE)
;
Linear Low Density (LLDPE)
;
Linear Low Density Polyethylene (LLDPE), Film Grade
;
LLDPE/Hexene, Film Grade
Material Notes:
A hexane linear low density polyethylene
Typical Applications:
Agricultural film
Cast film
Diaper backsheet
Overwrap film
Features:
Barefoot
High strength and stiffness
Good tensile and puncture resistance
Information provided by Southern Polymer
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Density
0.942
g/cc
Melt Flow
4.3
g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
Mechanical Properties
Original Value
Comments
Film Tensile Strength at Yield, MD
2350
psi
ASTM D882
Film Tensile Strength at Yield, TD
2480
psi
ASTM D882
Film Elongation at Break, MD
590 %
ASTM D882
Film Elongation at Break, TD
830 %
ASTM D882
Puncture Energy
7.00
in-lb
Elmendorf Tear Strength MD
20
g
ASTM D1922
Elmendorf Tear Strength TD
170
g
ASTM D1922
Dart Drop Test
<=
49.0
g
ASTM D1709A
Film Tensile Strength at Break, MD
7330
psi
ASTM D882
Film Tensile Strength at Break, TD
4950
psi
ASTM D882
1% Secant Modulus, MD
55300
psi
ASTM D882
1% Secant Modulus, TD
62300
psi
ASTM D882
Thermal Properties
Original Value
Comments
Melting Point
261
°F
Peak
Optical Properties
Original Value
Comments
Haze
3.4 %
ASTM D1003
Gloss
82 %
45°; ASTM D2457
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
PSOUTH047 / 283903
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.