MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Lord Adhesives Thermoset™ MD-150 Conductive Adhesive
Categories: Polymer; Adhesive

Material Notes: LORD Thermoset™ MD-150 silver-filled conductive adhesive offers excellent electrical and thermal conductivity. It is designed for use with automated dispensing, stamping and screen-printing application equipment.

Thermoset MD-150 adhesive provides excellent adhesion to a wide variety of surfaces including silicon, silver, gold and copper. Low ionic levels make it ideally suited for demanding semiconductor and hybrid assembly applications.

All information provided by Lord.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 3.50 g/cc
Viscosity 10000 cP
@Temperature 25.0 °C
 
Mechanical PropertiesOriginal ValueComments
Modulus of Elasticity 5.00 GPa
@Temperature 25.0 °C
Storage
Shear Strength 6000 psi
@Temperature 25.0 °C
Die
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 0.000080 ohm-cm
@Temperature 25.0 °C
 
Thermal PropertiesOriginal ValueComments
CTE, linear 54.0 µm/m-°CAlpha 1
 160 µm/m-°CAlpha 2
Glass Transition Temp, Tg 93.0 °CTMA
 
Processing PropertiesOriginal ValueComments
Cure Time 60.0 min
@Temperature 175 °C
Shelf Life 6.00 Month
@Temperature -40.0 °C
 
Component Elements PropertiesOriginal ValueComments
Potassium, K 0.0010 %
Sodium, Na 0.0050 %
 
Descriptive Properties
AppearanceSilver
Chloride (%)0.005
ConsistencyPaste

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Abatron 8509-2A/8509-1B Carbon-Filled Electrically Conductive Epoxy Compound
Epoxy Technology EPO-TEK® E2101 Electrically Conductive, Silver Epoxy
Master Bond EP51AN Thermally Conductive Adhesive System
Overview of materials for Silicone Rubber
Precision Polymer Engineering S70L Conductive Silicone Rubber

PLORD041 / 86049

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.