Deposit has good machinability and impact resistance, slightly harder than PF20. Excellent corrosion resistance. May be used for repairs to cast iron parts or overlay where nickel base alloy is required. Ametek has developed this and other engineering alloys for hardfacing - the process of spraying and fusing metal powder onto a work piece or substrate to give it specific hardness, wear, or corrosion resistant properties. Ametek® powders are engineered to have the precise size, spherical shape, and low oxygen content required for optimal thermal spraying characteristics. Information provided by Ametek Specialty Metal Products. |