MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Eagle Brass 200/201 Nickel Alloy, Annealed
Categories: Metal; Nonferrous Metal; Nickel Alloy

Material Notes: Nickel 200/201 has properties that are useful in industries such as chemical processing and electronics. Nickel is resistant to various reducing chemicals and alkaline materials. Compared with nickel alloys and many other materials 200/201 nickel has high electrical and thermal conductivity. It also has a high Curie temperature and good magnetostrictive properties. Annealed nickel has a low hardness and good ductility and formability. Those attributes, combined with good weldability, make the metal attractive for many types of parts.

Information provided by Eagle Brass Company

Key Words: ASTM B162
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.321 lb/in³As Annealed
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength >= 55.0 ksi
Elongation at Break >= 40 %in 2 inches
Tensile Modulus 30000 ksi
 
Thermal PropertiesOriginal ValueComments
CTE, linear 8.90 µin/in-°F
@Temperature 20.0 - 649 °C
Thermal Conductivity 306 BTU-in/hr-ft²-°F
 
Component Elements PropertiesOriginal ValueComments
Carbon, C <= 0.070 %
Iron, Fe <= 0.25 %
Manganese, Mn <= 0.35 %
Nickel, Ni >= 99.32 %Calculated as Balance
Sulfur, S <= 0.010 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Aperam Phyweld® 200 Bar-Corrosion application
ATI Allegheny Ludlum Stainless Steel Type 201, Annealed (UNS S20100)
Architectural Bronze, UNS C38500
Special Metals Nickel 201
AK Steel 201LN Austenitic Stainless steel

NEAGLE501 / 147481

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.