Alodine T 5900 treatment is a complex trivalent chromium conversion coating formulated for treating aluminum and its alloys, metals coated with IVD aluminum, magnesium, titanium and zinc surfaces. The process provides bare ASTM-B117 salt spray resistance, and it serves as an excellent base for bonding of paint and adhesives. Neither the product itself nor the conversion coating developed by the process contains hexavalent chromium. Alodine T 5900 can be used in immersion or pressure spray washers. |
Aerospace Surface Treatment |