MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Shanghai Potomer TYPE CR--232 CR2321 Chloroprene rubber
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: CR232 is a non-pollutant type chloroprene rubber of medium crystallization rate, a variety of general purpose rubber, made by polymerizing the emulsion with petroleum sodium sulfonate as disperser and non-sulfur modifier as modifier as modification agent, and similar to American Type W and Japanese Type M40 polychloroprene rubber.

Characteristics: CR232 is characterized by excellent storage stability, processability and safety property, and its products have sunlight resistance, oil resistance, chemical reagent resistance and combustion retardancy as well as heat resistance and less compression deformation. But its vulcanization rate is slow and should be solved by adjusting the vulcanization system

Application: CR232 can used for manufacturing oil-resistant rubber hose and rubber boards , cable jackets, rubber sealing parts, etc ,and is also widely used in making adhesive.

Information provided by Shanghai Potomer International Trade Co., Ltd

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Mooney Viscosity 35 - 45
@Temperature 100 °C
ML1+4
Ash <= 1.3 %
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength >= 14.7 MPa
Elongation at Break >= 700 %
Tensile Set <= 20.0 %
 
Descriptive Properties
Heating Loss<1.5%
Mooney scorch>13 minMS1+5, 120°C
Plasticity0.4-0.6

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSPOTOM040 / 284486

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.