Description: UNITHENE® LH606-13 is a high density polyethylene resin (HDPE) for use in injection molding. Characteristics: - Excellent weatherability
- Good environmental stress cracking resistance
- High impact strength
- Excellent stiffness
- High hardness
- Great surface gloss
- Less warpage
- Low shrinkage
Main Application: - Beer crates, fruit crates
- Food containers
- Pallets
Information provided by USI Corporation |