MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
LyondellBasell Lupolen 3721C High Density Polyethylene (HDPE), Blown Film Grade
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Film Grade

Material Notes: Lupolen 3721 C is a medium density polyethylene with hexene as comonomer. It exhibits a good processability and is used in stiff films and as blending component for LDPE. It contains antioxidants and is delivered in pellet form. This product is not intended for use in medical and pharmaceutical applications. Applications: Bags & Pouches, Food Packaging Film, Heavy Duty Packaging, Liner Film

Information provided by LyondellBasell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.937 g/ccISO 1183-1
Melt Flow 0.60 g/10 min
@Load 5.00 kg,
Temperature 190 °C
ISO 1133-1
 12.5 g/10 min
@Load 21.6 kg,
Temperature 190 °C
ISO 1133-1
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 20.0 MPaISO 527-1,-2
Film Elongation at Break, MD 650 %ISO 527-1,-3
Film Elongation at Break, TD 650 %ISO 527-1,-3
Tensile Modulus 700 MPaISO 527-1,-2
Dart Drop Test 120 gF50; ASTM D 1709
Film Tensile Strength at Break, MD 50.0 MPaISO 527-1,-3
Film Tensile Strength at Break, TD 48.0 MPaISO 527-1,-3
 
Thermal PropertiesOriginal ValueComments
Melting Point 127 °Cpeak; ISO 3146
Vicat Softening Point 121 °CA50N; ISO 306
 
Processing PropertiesOriginal ValueComments
Processing Temperature 180 - 240 °CExtrusion Temperature
 
Descriptive Properties
Failure Energy (J/mm)7DIN 53373
Processing MethodBlown Film
Test Specimenfilm, 20µm blown film extruded at 220°C, long stalk process and a blow up ratio 4:1

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
LyondellBasell Lupolen 3026F Low Density Polyethylene (LDPE), Blown Film Grade
LyondellBasell Lupolen 3010D Low Density Polyethylene (LDPE), Blow Molding Grade
Versalis Eraclene® FC 82 High Density Polyethylene - Blown Film Extrusion
Versalis Eraclene® FA 506 Hexene Copolymer High Density Polyethylene - Blown Film Extrusion
Versalis Flexirene® FG 30 U Butene Copolymer Linear Low Density Polyethylene

PEQT8554 / 220189

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.