MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
A. Schulman ComAlloy Voloy® 100 Polypropylene, Mineral Reinforced, Flame Retardant, UL, CSA
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Mineral Reinforced

Material Notes: Data provided by the manufacturer, ComAlloy International Company.

15% Mineral Reinforced.

The ComAlloy product line has been integrated into the A Schulman product line.

Key Words: ComAlloy International Company, subsidiary of A. Shulman Inc.
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.36 g/cc
Linear Mold Shrinkage 0.010 cm/cmASTM D955
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 96ASTM D785
Tensile Strength, Ultimate 27.0 MPaASTM D638
Elongation at Break 15 %ASTM D638
Flexural Strength 48.0 MPaASTM D790
Flexural Modulus 2.70 GPaASTM D790
Izod Impact, Notched 0.320 J/cmASTM D256
Izod Impact, Unnotched 2.67 J/cmASTM D256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 118 °CASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 74.0 °CASTM D648
 
Processing PropertiesOriginal ValueComments
Middle Barrel Temperature 210 - 221 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
LyondellBasell Hostacom HKC 1340D BLACK Polypropylene, Mineral Reinforced
ICO Polymers ICORENE™ 440-1312 PP Rotational Molding Resin
Cossa Polimeri ESTAPROP 1540 TG V0 H Flame Retardant Polypropylene, 20% Mineral Filled
A. Schulman ComAlloy® E-14756 Flame Retardant Easy Flow Polycarbonate Alloy
ExxonMobil PP1404FC Mineral-filled Homopolymer

PASH2W / 24867

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.