Notes: Sarlink EE-2300 series is a high performance thermoplastic elastomer series, available in BLK, designed for demanding automotive low gloss extrusion applications including functional lip seals. Sarlink EE-2375B is a medium hardness, high density, filled, UV stabilized grade with exceptional tensile strength, superior surface aesthetics, good chemical resistance and good elasticity. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North America Features: Chemical Resistant; Good Adhesion; Good Flexibility; Good Processability; Good Scratch Resistance; High Density; High Elasticity; High Melt Stability; High Specific Gravity; High Tensile Strength; Low Gloss; Medium Hardness; Outstanding Surface Finish; UV Resistant Uses: Automotive Applications; Automotive Exterior Parts; Profiles; Rubber Replacement; Seals; Weatherstripping RoHS Compliance: RoHS Compliant Form: Pellets Processing Method: Extrusion Preliminary data. Information provided by Teknor Apex |