MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
ThyssenKrupp XABO® 355 T Structural Steel
Categories: Metal; Ferrous Metal; Carbon Steel; Low Carbon Steel

Material Notes: This Material Specification applies to thermomechanically rolled flat products in thicknesses up to 60 mm. The criteria to distinguish the steel grades is the lowest test temperature for the notch-bar impact test.

Application: The steels are applied in welded constructions such as supporting structures, vessels etc., where a secured preventin against cold cracking in the welded joints is required. Due to the low carbon equivalent, these steels are highly resistant against cold cracking.

Information Provided by Thyssen Krupp

Key Words: S335ML; EN 1.8834
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 7.85 g/cc
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 450 - 600 MPa
Tensile Strength, Yield >= 335 MPa35
 >= 345 MPa
@Thickness 16.0 - 35.0 mm
 >= 355 MPa
@Thickness 16.0 mm
Elongation at Break >= 22 %
Modulus of Elasticity 213 GPa
Charpy Impact 16.0 J
@Temperature -50.0 °C
Transverse
 25.0 J
@Temperature -40.0 °C
Transverse
 27.0 J
@Temperature -50.0 °C
Longitudinal
 35.0 J
@Temperature -30.0 °C
Transverse
 40.0 J
@Temperature -40.0 °C
Longitudinal
 45.0 J
@Temperature -20.0 °C
Transverse
 50.0 J
@Temperature -30.0 °C
Longitudinal
 65.0 J
@Temperature -20.0 °C
Longitudinal
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 0.000030 ohm-cm
 
Thermal PropertiesOriginal ValueComments
Specific Heat Capacity 0.450 J/g-°C
Thermal Conductivity 45.0 W/m-K
 
Component Elements PropertiesOriginal ValueComments
Carbon, C <= 0.13 %
Iron, Fe >= 97 %As Balance
Manganese, Mn <= 1.6 %
Nickel, Ni <= 0.30 %
Niobium, Nb (Columbium, Cb) <= 0.050 %
Other <= 0.39 %Carbon Equivalent
Phosphorus, P <= 0.025 %
Silicon, Si <= 0.50 %
Sulfur, S <= 0.010 %
 
Descriptive Properties
Magnetic Propertiesmagnetizable
Thermal diffusivity (cm²/s)0.13

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
ThyssenKrupp XABO® 355 Structural Steel
ThyssenKrupp PAS 355 Structural Steel for Cold Forming
AM-355 Stainless Steel Plate, Sheet, Strip, Condition H850, UNS S35500
Aluminum 6061-T6; 6061-T651
AM-355 Stainless Steel Forgings, Condition H1000, UNS S35500

NTHYSS035 / 90355

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.