MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
LG Chemical LUMAX GP5106FI PBT+ABS+GF10%, Flame Retardant
Categories: Polymer; Thermoplastic; ABS Polymer; Acrylonitrile Butadiene Styrene (ABS), 10% Glass Fiber Filled; Polyester, TP; Polybutylene Terephthalate (PBT); Polybutylene Terephthalate (PBT), 10% Glass Fiber Filled; Polybutylene Terephthalate (PBT), Flame Retardant

Material Notes: Description: Injection Molding Grade, PBT+ABS+GF10%, Flame Retardant, Impact Modified, Dimensional Stability

Application: E&E (Switch)

CAS: 9003-56-9, 68928-70-1, 65997-17-3, 24968-12-5, 9003-54-7 and 1309-64-4

Information provided by LG Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.40 g/ccASTM D792
Maximum Moisture Content 0.020Injection Molding
Linear Mold Shrinkage, Flow 0.0040 - 0.0090 cm/cm
@Thickness 3.20 mm
ASTM D955
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 570 kg(f)/cm²
@Thickness 3.20 mm
5mm/min; ASTM D638
Elongation at Break 3.0 %
@Thickness 3.20 mm
5mm/min; ASTM D638
Flexural Yield Strength 850 kg(f)/cm²
@Thickness 3.20 mm
1.3mm/min; ASTM D790
Flexural Modulus 30000 kg(f)/cm²
@Thickness 3.20 mm
1.3mm/min; ASTM D790
Izod Impact, Notched 6.00 kg-cm/cm
@Thickness 3.20 mm,
Temperature 23.0 °C
ASTM D256
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+15 ohm-cmASTM D257
Dielectric Strength 26.0 kV/mm
@Thickness 1.00 mm
ASTM D149
Arc Resistance 60 - 120 secASTM D495
Comparative Tracking Index 175 VSolution A; IEC 60112
Hot Wire Ignition, HWI 15 - 30 sec
@Thickness >=1.50 mm
 30 - 60 sec
@Thickness >=3.00 mm
High Amp Arc Ignition, HAI 30 - 60 arcs
@Thickness 3.00 mm
 60 - 120 arcs
@Thickness 1.50 mm
High Voltage Arc-Tracking Rate, HVTR >= 150 mm/min
 
Thermal PropertiesOriginal ValueComments
Melting Point 225 °CPeak at Break
Deflection Temperature at 1.8 MPa (264 psi) 110 °C
@Thickness 6.40 mm
Unannealed; ASTM D648
UL RTI, Electrical 60.0 °C
@Thickness >=1.50 mm
 60.0 °C
@Thickness >=3.00 mm
UL RTI, Mechanical with Impact 60.0 °C
@Thickness >=1.50 mm
 60.0 °C
@Thickness >=3.00 mm
UL RTI, Mechanical without Impact 60.0 °C
@Thickness >=1.50 mm
 60.0 °C
@Thickness >=3.00 mm
Flammability, UL94 V-0
@Thickness >=1.50 mm
 V-0
@Thickness >=3.00 mm
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 225 - 235 °CInjection Molding
Middle Barrel Temperature 230 - 245 °CInjection Molding
Front Barrel Temperature 240 - 250 °CInjection Molding
Nozzle Temperature 240 - 250 °CInjection Molding
Melt Temperature 240 - 250 °CInjection Molding
Mold Temperature 60.0 - 90.0 °CInjection Molding
Drying Temperature 100 °CInjection Molding
Dry Time 4.00 - 5.00 hourInjection Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Mid-Mountain Materials ARMATEX® SF7 Silicone Rubber Coated Glass Fabric

PLAY451 / 148461

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.