(Viewing data as-entered.
Click here
to return)
UBE UBEPOL BR150 Non-Oil Extended Synthetic Rubber (Raw Polymer)
Categories:
Polymer
;
Thermoset
;
Rubber or Thermoset Elastomer (TSE)
Material Notes:
Description:
UBEPOL BR is UBE's line of polybutadiene rubber products. Stabilizer Type: Non-staining
Microstructure:
cis: 98
trans: 1
vinyl: 1
Information provided by UBE.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Density
0.910
g/cc
ASTM D1505
Volatiles
0.30 %
ASTM D1416
Viscosity
75
cP
@Temperature 25.0 °C
Solution Viscosity in 5 wt.% Toluene; UBE Method
Viscosity Measurement
2.1
@Temperature 30.0 °C
Intrinsic Viscosity in Toluene; UBE Method
Mooney Viscosity
43
@Temperature 100 °C
ML1+4; ASTM D1646
Molecular Weight
560000
g/mol
No units specified (Number Average Molecular Weight (10^4) = 20); UBE Method
Ash
0.050 %
ASTM D1416
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
Users viewing this material also viewed the following:
Chi Mei Kibipol® PR-1205 Butadiene Rubber (SSBR)
ZEON Nipol® 1042 Nitrile Elastomer
ZEON Nipol® 1052 Nitrile Elastomer
Dow BETAPHON™ 2 Synthetic Rubber
Natural Rubber, Vulcanized (NR, IR, Polyisoprene)
PUBE172 / 71732
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.