Hifax polypropylene resins based on the Catalloy process are used in applications such as building and construction (e.g., single-ply roofing), industrial applications (e.g., wire and cable), and automotive industries. Hifax priovides good processability, excellent impact resistance, a broad range of stiffness from very soft to rigid products, high temperature resistance and low linear coefficient of thermal expansion. Hifax CA 7320 A is a reactor TPO (thermoplastic polyolefin) manufactured using the LyondellBasell’s proprietary Catalloy process technology. It is designed for use in compounds where it shows high efficiency as impact modifier. It gives excellent processability whilst maintaining optimum mechanical properties. The grade is available in natural pellet form. Applications: Impact Modification, Polymer Modifier. Information provided by LyondellBasell. |