MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Envalior Pocan® B 4235 000000 PBT, 30% Glass Fiber
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); Polybutylene Terephthalate (PBT), 30% Glass Fiber Filled

Material Notes: PBT, 30% glass fibers, injection molding, flame retardant

Former Lanxess product line is now with Envalior.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.65 g/ccISO 1183
Water Absorption 0.40 %Test Sim. to ISO 62
Moisture Absorption at Equilibrium 0.10 %23°C/50% R.H.; Test Sim. to ISO 62
Viscosity Number 93 cm³/gISO 307, 1157, 1628
Linear Mold Shrinkage, Flow 0.0040 cm/cmISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.0010 cm/cmISO 294-4, 2577
Melt Flow 20 g/10 min
@Load 2.16 kg,
Temperature 260 °C
Calculated from MVR using melt density; ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 134 MPaISO 527-1/-2
Elongation at Break 2.2 %ISO 527-1/-2
 2.9 %Nominal; ISO 527-1/-2
Tensile Modulus 10300 MPaISO 527-1/-2
Charpy Impact Unnotched 50.0 kJ/m²
@Temperature -30.0 °C
ISO 179/1eU
 50.0 kJ/m²
@Temperature 23.0 °C
ISO 179/1eU
Charpy Impact, Notched <= 10.0 kJ/m²
@Temperature -30.0 °C
ISO 179/1eA
 <= 10.0 kJ/m²
@Temperature 23.0 °C
ISO 179/1eA
Impact 661Puncture maximum force (N); ISO 6603-2
Puncture Energy 2.30 JISO 6603-2
Tensile Creep Modulus, 1 hour 11000 MPaISO 899-1
Tensile Creep Modulus, 1000 hours 10000 MPaISO 899-1
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+15 ohm-cmIEC 60093
Surface Resistance >= 1.00e+15 ohmIEC 60093
Dielectric Constant 3.9
@Frequency 1e+6 Hz
IEC 60250
 4.0
@Frequency 100 Hz
IEC 60250
Dielectric Strength 29.0 kV/mmIEC 60243-1
Dissipation Factor 0.0050
@Frequency 100 Hz
IEC 60250
 0.016
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 175 VIEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 20.0 µm/m-°CISO 11359-1/-2
CTE, linear, Transverse to Flow 80.0 µm/m-°CISO 11359-1/-2
Melting Point 225 °C10°C/min; ISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 220 °CISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 210 °CISO 75-1/-2
Deflection Temperature at 8.0 MPa 130 °CISO 75-1/-2
Vicat Softening Point 210 °C50°C/h 50N; ISO 306
Flammability, UL94 V-2
@Thickness 0.800 mm
IEC 60695-11-10
 V-0
@Thickness 1.60 mm
IEC 60695-11-10
 5VA
@Thickness 3.20 mm
IEC 60695-11-20
Oxygen Index 32 %ISO 4589-1/-2
 
Processing PropertiesOriginal ValueComments
Melt Temperature 260 °CInjection Molding; ISO 294
Mold Temperature 80.0 °CInjection Molding; ISO 10724
 
Descriptive Properties
AdditivesFlame retarding agent
 Release agent
FeaturesFlame retardant
FormPellets
ISO Short NameISO 7792-1-PBT,GFHMR,09-100;GF30; ISO 1043-PBT GF FR(17)
ProcessingInjection molding
RegionAsia Pacific
 Europe
 Near East/Africa
 North America
 South and Central America

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
BASF Ultradur® B 4406 G6 30% Glass Filled PBT
Envalior Pocan® B 3235 000000 PBT, 30% Glass Fiber
A. Schulman ComAlloy Voloy® 431 Glass/Mineral Reinforced, PET Alloy, Flame Retardant, UL
Covestro Makrolon® GF8001 Polycarbonate, 20% Glass Filled
BASF Ultradur® B 4300 G6 30% Glass Filled PBT

PLANX0862 / 99077

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.