NatureWorks® PLA polymer 6350D is an amorphous thermoplastic spunbond-grade resin derived primarily from annually renewable resources. Available in pellet form, 6350D is designed for extrusion into spunbond nonwovens using conventional bi-component PET spunbond equipment, where filament velocities > 4000 m/min can be achieved. NatureWorks® PLA 6350D can be used as a low melt binder polymer in a sheath-core configuration. Potential applications for PLA polymer 6350D include bicomponent spunbond non-wovens |