Glass Fiber Reinforced grades-10% glass fiber, flame resistant grade, Non-Bromine / non-phosphorus, weather resistant. Availability: Africa, Middle East, Asia Pacific, Europe, Latin America, North America. Filter / reinforcement: Glass fiber, 10% filler by weight. Features: Bromine Free, Creep resistant, flame resistant, High Ridigity, High flow, Low (to none) phosphorus content, weather resistant. Uses: Electrical parts, Electrical / electronic applications, industrial applications. Forms: pellets. Processing Method: Injection Molding.Information provided by Teijin Chemicals Ltd. |