MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Domo TECHNYL® A 218HP V50 PA66, 35% glass fiber, DRY
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 40% Glass Fiber Filled

Material Notes: Description: TECHNYL® A 218HP V50 is a polyamide 66, reinforced with 50% of glass fiber, heat stabilized, for injection molding. This product is available in black color.

Benefits: The product offers an outstanding long term heat resistance and is suitable to work in environments characterized by a very high temperature.

Available in: Asia Pacific, Europe and Latin America

Regulations compliance: Grades produced or imported in Europe comply with directive 453/2010/EC, which amends REACH directive 1907/2006/EC. This grade complies with RoHS directive 2002/95/EC. Unless specified, this grade is not suitable for food contact, medical devices or toy applications.

Applications: It is used in a wide variety of industries, especially in automotive industry for air circuit parts such as intercoolers.

DOMO Chemicals has acquired Solvay’s Performance Polyamides Business in Europe.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.52 g/ccISO 1183/A
Linear Mold Shrinkage 0.0060 cm/cmIsotropy
Linear Mold Shrinkage, Flow 0.0030 cm/cm
Linear Mold Shrinkage, Transverse 0.0050 cm/cm
 0.0090 cm/cmISO 294-4
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 200 MPaISO 527 Type 1A
Tensile Stress at Strain 39.0 MPa
@Strain 1 %,
Temperature 200 °C
 45.0 MPa
@Strain 2 %,
Temperature 200 °C
 48.0 MPa
@Strain 3 %,
Temperature 200 °C
 50.0 MPa
@Strain 4 %,
Temperature 200 °C
 80.0 MPa
@Strain 0.5 %,
Temperature 23.0 °C
 150 MPa
@Strain 1 %,
Temperature 23.0 °C
 180 MPa
@Strain 1.5 %,
Temperature 23.0 °C
Elongation at Break 2.0 %ISO 527 Type 1A
Tensile Modulus 15000 MPaISO 527 Type 1A
Flexural Strength 280 MPaASTM D790
 320 MPaISO 178
Flexural Modulus 13500 MPaISO 178
 13500 MPaASTM D790
Izod Impact, Notched (ISO) 20.0 kJ/m²ISO 180/1eA
Izod Impact, Unnotched (ISO) 80.0 kJ/m²ISO 180/1eU
Charpy Impact Unnotched 85.0 kJ/m²ISO 179/1eU
Charpy Impact, Notched 17.0 kJ/m²ISO 179/1eA
 
Thermal PropertiesOriginal ValueComments
Melting Point 263 °CISO 11357
Deflection Temperature at 0.46 MPa (66 psi) 260 °CISO 75/Bf
Deflection Temperature at 1.8 MPa (264 psi) 253 °CISO 75/Af
Flammability, UL94 HB
@Thickness 0.800 mm
1210
 HB
@Thickness 1.60 mm
1210
 HB
@Thickness 3.20 mm
1210
 
Processing PropertiesOriginal ValueComments
Feed Temperature 265 - 275 °C
Mold Temperature 80.0 - 110 °C
Drying Temperature 80.0 °C
Moisture Content <= 0.12 %
 
Descriptive Properties
Compression Zone270-280°C
Mixing Zone280-290°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Domo TECHNYL® A 218 V50 PA66, 50% glass fiber, DRY
Domo TECHNYL® A 218 PA66, 33% glass fiber, DRY
Domo TECHNYL® A 218 V35 PA66, 35% glass fiber, DRY
Domo TECHNYL® A 218W V30 Natural PA66, 30% glass fiber, DRY
Muntz metal, UNS C28000, H02 Temper flat products

PRHOD674 / 137905

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.