MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

(Viewing data as-entered. Click here to return)
Henkel Loctite® 409 General Purpose Ethyl Cyanoacrylate Bonding Adhesive
Categories: Polymer; Adhesive; Thermoset; Acrylic/Cyanoacrylate Adhesive

Material Notes:
Cyanoacrylate Bonding Adhesives
Loctite® technology has made the productivity promises of cyanoacrylate adhesives a reality with the industry's widest selection of high-performance, application-specific, instant adhesives. Loctite® Instant Adhesives are available in a variety of viscosities, cure speeds, gap-filling capability and substrate compatibility. The ultra high-performance PRISM® family offers additional products that surpass the most stringent demands, including toughened formulations, low odor and low blooming products, surface insensitive and thermally resistant formulations.

Loctite® 409 General Purpose Ethyl Cyanoacrylate Bonding Adhesive
Cure Type: 5950 Bonding Type: Cyanoacrylate Typical Use: General purpose gel adhesive

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.10 g/cc
 
Mechanical PropertiesOriginal ValueComments
Adhesive Bond Strength 3200 psiGrit blasted steel
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 180 °F
Minimum Service Temperature, Air -65.0 °F
 
Processing PropertiesOriginal ValueComments
Cure Time 1.25 min
 24.0 hourFull Cure; Varies with substrates
 
Descriptive Properties
ColorClear
Gap Fill0.01 in.
ViscosityGel

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Henkel Loctite® 420 General Purpose Ethyl Cyanoacrylate Bonding Adhesive
Henkel Loctite® 417 General Purpose Ethyl Cyanoacrylate Bonding Adhesive
Henkel Loctite® 416 General Purpose Ethyl Cyanoacrylate Bonding Adhesive
Henkel Loctite® 414 General Purpose Ethyl Cyanoacrylate Bonding Adhesive
Henkel Loctite® 412 General Purpose Ethyl Cyanoacrylate Bonding Adhesive

PLOCT017 / 51753

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.