MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

USP Class VI Adhesives
USP Class VI Approved Adhesives for Medical Device Applications
Master Bond’s biocompatible adhesives are designed to meet the needs of medical device manufacturers. Compounds withstand various types of sterilization methods.

(Viewing data as-entered. Click here to return)
Henkel Loctite® FLASHCURE™ 4303 Light Cure Instant Adhesive
Categories: Polymer; Adhesive; Thermoset; Acrylic/Cyanoacrylate Adhesive

Material Notes:
Cyanoacrylate Light Cure Adhesives
Loctite offers the most comprehensive line of adhesives and sealants available to the medical device industry. These USP class VI and/or ISO-10993 compliant products are designed specifically for the assembly of medical devices where toxicity testing and sterilization resistance are required.

Loctite® 4303 FLASHCURE™ Light Cure Instant Adhesive
New patented technology. Two component, low or high viscosity. Specifically formulated for extremely rapid UV or visible light cure and secondary cyanoacrylic cure mechanism. Eliminates the need for solvent-based accelerators. Surface versatile. Key Substrates: Elastomer, metal, polycarbonate, thermoplastic Cure Type: Ultraviolet, Visible, Moisture Bonding Type: Cyanoacrylate

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Brookfield Viscosity 900 cP
@Temperature 25.0 °C
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 65
Elongation at Break 2.0 %
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 250 °F
Minimum Service Temperature, Air -65.0 °F
 
Descriptive Properties
ColorLight amber/faint green

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PLOCT084 / 51820

USP Class VI Adhesives
USP Class VI Approved Adhesives for Medical Device Applications
Master Bond’s biocompatible adhesives are designed to meet the needs of medical device manufacturers. Compounds withstand various types of sterilization methods.

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.