MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
LyondellBasell Hostalen PP XN125-P Polypropylene Copolymer
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene Copolymer

Material Notes: Hostalen PP XN125-P is a natural colored polypropylene random copolymer. The product Hostalen PP XN125-P has been classified through ISO9080 and according to ISO12162 as PP125. The regression curves of Hostalen PP XN125-P are above the reference lines of PP-RCT mentioned in DIN8077, DIN 8078 and EN ISO15874 standards for piping applications under pressure. Hostalen PP XN125-P is typically used in the application pressure piping systems for hot and cold water. Applications: Drinking Water Pipe, Plumbing, Heating & Cooling

Information provided by LyondellBasell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.905 g/ccISO 1183-1
Oxidative Induction Time (OIT) 40 min
@Temperature 210 °C
ISO 11357-6
Melt Flow 0.20 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ISO 1133-1
 0.55 g/10 min
@Load 5.00 kg,
Temperature 190 °C
ISO 1133-1
 1.1 g/10 min
@Load 5.00 kg,
Temperature 230 °C
ISO 1133-1
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 26.0 MPaISO 527-1,-2
Elongation at Break 400 %ISO 527-1,-2
Elongation at Yield 12 %ISO 527-1,-2
Tensile Modulus 850 MPaISO 527-1,-2
Charpy Impact, Notched 2.00 kJ/m²
@Temperature -20.0 °C
ISO 179-1/1eA
 8.00 kJ/m²
@Temperature 0.000 °C
ISO 179-1/1eA
 60.0 kJ/m²
@Temperature 23.0 °C
ISO 179-1/1eA
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 70.0 °Cunannealed; ISO 75B-1,-2
DSC Induction Temperature 136 °CDSC
 
Descriptive Properties
MRS Classification (MPA)12.5ISO 9080
Processing Methodinjection molding, pipe

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Borealis RA7050-GN Polypropylene-Random-Copolymer for Pressure Pipe Systems
Total PPR 8650 Polypropylene, Random Copolymer
LyondellBasell Hostalen PP XN112-I Polypropylene Copolymer
LyondellBasell Hostalen PP H5416 Polypropylene Copolymer
Ascend Performance Materials Starflam® M10009AP PP, Flame Retardant, Injection Molding

PEQT8522 / 220157

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.