MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Eurotec® Tecodur® PB70 GR20 BK002 TD21 PBT/PET, 20% glass fiber reinforced, flame retardant - halogen (RoHS compliant), impact modified, natural
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); PBT + PET Blend, Glass Filled; Polybutylene Terephthalate (PBT), Impact Grade; Polyethylene Terephthalate (PET)

Material Notes:

Information provided by Eurotec®

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.52 g/ccISO 1183
Moisture Absorption 0.200 %
@Temperature 23.0 °C
50% RH; ISO 960
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 100 MPaISO 527
Elongation at Break 3.0 %ISO 527
Tensile Modulus 7500 MPaISO 527
Izod Impact, Notched (ISO) 9.00 kJ/m²
@Temperature -30.0 °C
ISO 180/1A
 10.0 kJ/m²
@Temperature 23.0 °C
ISO 180/1A
Izod Impact, Unnotched (ISO) 60.0 kJ/m²
@Temperature -30.0 °C
ISO 180/1U
 65.0 kJ/m²
@Temperature 23.0 °C
ISO 180/1U
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+16 ohm-cmIEC 60093
Surface Resistance 1.00e+14 ohmIEC 60093
Comparative Tracking Index 225 VSolution A; IEC 60112
 
Thermal PropertiesOriginal ValueComments
Melting Point 225 - 255 °C[10 K/min], ISO 11357
Deflection Temperature at 0.46 MPa (66 psi) 215 °CISO 75
Deflection Temperature at 1.8 MPa (264 psi) 175 °CISO 75
Flammability, UL94 V-2
@Thickness 0.750 mm
 V-0
@Thickness 1.60 mm
Glow Wire Ignition Temperature 725 °C
@Thickness 2.00 mm
IEC 60695
Glow Wire Flammability Index 960 °C
@Thickness 2.00 mm
IEC 60695
 
Processing PropertiesOriginal ValueComments
Processing Temperature 240 - 270 °C
Feed Temperature 50.0 - 70.0 °CThroat
Mold Temperature 60.0 - 110 °C
Drying Temperature 120 °C
Dry Time 2.00 - 4.00 hour
Moisture Content <= 0.080 %ISO 960
Hold Pressure 40.0 - 80.0 MPa
 
Descriptive Properties
Back PressureLow
Injection SpeedMedium - Fast

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Polyplastics Duranex® 7390W Polybutylene Terephthalate (PBT), Super low warpage, GF filled
DSM Arnite® TV4 440 KL PBT/PET Blend-20% Glass Reinforced (European Grade)
BASF Ultradur® B 4040 G6 High Speed BK15029 30% Glass Filled PBT/PET
BASF Ultradur® B 4040 G4 20% Glass Filled PBT + PET
BASF Ultradur® B 4040 G10 50% Glass Filled BK 15029 PBT + PET

PEUROS126 / 147116

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.