MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Crucible Steel HALGRAPH® Tool Steel, AISI O6
Categories: Metal; Ferrous Metal; Tool Steel; Oil-Hardening Steel

Material Notes: Halgraph is an oil-hardening graphitic tool steel with excellent non-deforming properties. Free graphite in its structure affords exceptional free-machining properties. The combination of graphite and hard carbides give Halgraph tools excellent resistance to adhesive wear (galling) in applications such as ring gauges, plug gauges, and bushings.

Information provided by Crucible Industries

Key Words: AISI O6
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.278 lb/in³
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 187 - 221
Hardness, Rockwell C 64 - 66hardened at 1475°F then quenched
 45 - 47
@Tempering Temp. 482 °C
hardened at 1475F then tempered
 49 - 51
@Tempering Temp. 427 °C
hardened at 1475F then tempered
 53 - 55
@Tempering Temp. 371 °C
hardened at 1475F then tempered
 55 - 57
@Tempering Temp. 343 °C
hardened at 1475F then tempered
 57 - 59
@Tempering Temp. 288 °C
hardened at 1475F then tempered
 57 - 59
@Tempering Temp. 316 °C
hardened at 1475F then tempered
 58 - 60
@Tempering Temp. 260 °C
hardened at 1475F then tempered
 59 - 61
@Tempering Temp. 232 °C
hardened at 1475F then tempered
 60 - 62
@Tempering Temp. 204 °C
hardened at 1475F then tempered
 61 - 63
@Tempering Temp. 177 °C
hardened at 1475F then tempered
 62 - 64
@Tempering Temp. 149 °C
hardened at 1475F then tempered
Modulus of Elasticity 30000 ksi
Charpy Impact 20.0 ft-lb
@Tempering Temp. 149 °C
hardened at 1475°F then tempered; C-notch
 20.0 ft-lb
@Tempering Temp. 260 °C
hardened at 1475°F then tempered; C-notch
 27.0 ft-lb
@Tempering Temp. 204 °C
hardened at 1475°F then tempered; C-notch
 27.0 ft-lb
@Tempering Temp. 316 °C
hardened at 1475°F then tempered; C-notch
 35.0 ft-lb
@Tempering Temp. 371 °C
hardened at 1475°F then tempered; C-notch
 42.0 ft-lb
@Tempering Temp. 427 °C
hardened at 1475°F then tempered; C-notch
 53.0 ft-lb
@Tempering Temp. 482 °C
hardened at 1475°F then tempered; C-notch
 
Thermal PropertiesOriginal ValueComments
CTE, linear 6.20 µin/in-°F
@Temperature 21.1 - 204 °C
 6.70 µin/in-°F
@Temperature 21.1 - 316 °C
 7.10 µin/in-°F
@Temperature 21.1 - 427 °C
Thermal Conductivity 34.5 W/m-K
@Temperature 95.0 °C
 
Processing PropertiesOriginal ValueComments
Processing Temperature 1385 °FCritical Thermal Treatment Temperature
 
Component Elements PropertiesOriginal ValueComments
Carbon, C 1.5 %
Iron, Fe 96.45 %as balance
Manganese, Mn 0.75 %
Molybdenum, Mo 0.30 %
Silicon, Si 1.0 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Carpenter O6 Graphitic Tool Steel (AISI O6)
AISI Type O6 Tool Steel
Crucible Steel KETOS® Tool Steel, AISI O1
AISI Type O1 Oil-hardening Tool Steel, oil quenched at 800°C, tempered at 425°C
ATI Allegheny Ludlum 06 Tool Steel, UNS T31506

NCRUC914 / 160365

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.