MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Avient Edgetek® XT XT-100-BW00 Natural Polycarbonate + PBT (PC+PBT)
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Unreinforced; Polyester, TP; Polybutylene Terephthalate (PBT); Polybutylene Terephthalate (PBT), Unreinforced, Molded

Material Notes: EDGETEK™ XT High Performance Polymers are polycarbonate and polyester alloys that combine strength, durability and chemical resistance. The Edgetek XT product family includes a complete line of general purpose, UV stable and low-temperature impact grades for use in a wide range of demanding applications and severe operating environments plus customized formulations to meet specialized requirements.

Information provided by PolyOne

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.20 g/ccASTM D792
Linear Mold Shrinkage, Flow 0.0060 - 0.0080 cm/cmASTM D955
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 56.5 MPaType I, 5.1 mm/min; ASTM D638
Elongation at Break 120 %Type I, 5.1 mm/min; ASTM D638
Flexural Strength 82.7 MPaASTM D790
Flexural Modulus 2170 MPaASTM D790
Izod Impact, Notched 210 J/m
@Thickness 3.18 mm,
Temperature -20.0 °C
Injection Molded; ASTM D256A
 800 J/m
@Thickness 3.18 mm,
Temperature 23.0 °C
Injection Molded; ASTM D256A
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 105 °C
@Thickness 6.35 mm
Unannealed; ASTM D648
 
Processing PropertiesOriginal ValueComments
Melt Temperature 260 - 277 °C
Mold Temperature 65.6 - 87.8 °C
Drying Temperature 110 °C
Dry Time 2.00 hour
 
Descriptive Properties
FeaturesGood Weather Resistance
FormsPellets
Generic MaterialPC+PBT
Generic NamePolycarbonate + PBT (PC+PBT)
Regional AvailabilityAfrica & Middle East
 Asia Pacific
 Europe
 North America
 South America

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
A. Schulman Lucent PC/PBT-1550 Polycarbonate+PBT, Improved Impact Resistance, Injection Grade
Avient Edgetek® XT EX3600-0002 UV Black Polycarbonate + PBT (PC+PBT)
Avient Edgetek® XT XT-500-CU00 Polycarbonate + PBT (PC+PBT)
A. Schulman Lucent PC/PBT-1830 Polycarbonate+PBT, Superior Cold Temp Impact, Injection Grade
Covestro Makroblend® UT4045 G PC/PBT Blend, 20% Glass Filled

PH0POL0716 / 145285

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.