MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Cadi 182 Copper Alloy
Categories: Metal; Nonferrous Metal; Copper Alloy

Material Notes: Chromium copper is the primary copper alloy used for resistance spot and seam welding. This alloy achieves good hardness and electrical conductivity through a combination of heat treatment and cold work. C18200 is utilized for electrodes, holders, adaptors, as well as numerous electrical applications where resistance to deformation at high temperature is required or when higher mechanical properties than C11000 are required.

Forms:

  • Rod
  • Bar
  • Plate
  • Shapes
  • Tube

Information provided by Cadi Company.

Key Words: MIL-C-19311B, UNS C18200
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 8.89 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell B 65
@Diameter 50.8 - 76.2 mm
 70
@Diameter 25.4 - 50.8 mm
 >= 75
@Diameter <=25.4 mm
heat treated
Tensile Strength at Break >= 55000 psiAny thickness
Tensile Strength, Yield >= 55000 psi
@Strain 0.5 %
Any thickness
Modulus of Elasticity 17000 ksi
Poissons Ratio 0.181
Shear Modulus 7200 ksi
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity <= 0.00000382 ohm-cm>75% IACS, up to 3" diameter/any thickness
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 2244 BTU-in/hr-ft²-°F
Melting Point 1958 - 1976 °F
Solidus 1958 °F
Liquidus 1976 °F
 
Processing PropertiesOriginal ValueComments
Processing Temperature 1200 °FBrazing, <15 minutes
 
Component Elements PropertiesOriginal ValueComments
Chromium, Cr 0.90 %
Copper, Cu 99.1 %
 
Descriptive Properties
RMWA Class2

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Eagle Brass 101 OFE COPPER (Certified), Hard
Eagle Brass 110 EPT COPPER, 1/2 Hard
Ampco Metal AMPCOLOY® 972 Chromium-Copper Alloy, Extruded and Drawn Rods, 10 - 25 mm.
IBC Advanced Alloys C18150 Chrome Copper Zirconium Alloy, TL06 Temper
Chromium Copper, UNS C18200, TB00 Temper rod

NCADI12 / 15520

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.