Notes: Telcar TL-3954-62 is a general purpose thermoplastic elastomer designed for a variety of wire and cable applications, including cable jacketing and cable insulation. Telcar TL-3954-62 is a medium hardness, high density grade that is RoHS compliant grade that is suitable for both injection molding and extrusion. Features: Filled; General Purpose; Good Mold Release: Good Moldability; Good Processability; High Density; High Specific Gravity; Low Flow; Medium Hardness Uses: Appliance Wire Insulation; Appliance Wire Jacketing; Cable Jacketing; Connectors; Construction Applications; Flexible Cord Jacketing; Industrial Applications; Industrial Cable Insulation; Terminal Cable Jacketing; Underground Power Cable; Wire and Cable Applications; Wire Jacketing Forms: Pellets Processing Method: Extrusion; Injection Molding Injection Notes: Injection Rate: Moderate-Fast Extrusion Notes: Screw Speed: 30 to 100 rpm Information Provided by Teknor Apex |