MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
A. Schulman Diamond NPP10-0105 Vinyl Acetate Copolymer
Categories: Polymer; Thermoplastic; Polyethylene (PE); Low Density (LDPE)

Material Notes:

A. Schulman has acquired Network Polymers & Diamond Polymers.

Key Words: Low Density Polyethylene
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.925 g/ccASTM D1505
Vinyl Acetate Content 4.6 %
Melt Flow 1.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 24.7 MPaTransverse to Flow; ASTM D882
 25.9 MPaDirection of Flow; ASTM D882
Elongation at Break 180 %Direction of Flow; ASTM D882
 580 %Transverse to Flow; ASTM D882
Dart Drop, Total Energy 190 JF50; ASTM D1790
Tear Strength Test 90g; Transverse to Flow; ASTM D1922
 200g; Direction of Flow; ASTM D1922
1% Secant Modulus, MD 146 MPaASTM D882
1% Secant Modulus, TD 168 MPaASTM D882
 
Thermal PropertiesOriginal ValueComments
Vicat Softening Point 89.0 °CASTM D1525
 
Optical PropertiesOriginal ValueComments
Haze 6.4 %ASTM D1003
Gloss 71 %45°; ASTM D2457

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Hydrogenated Nitrile Rubber (HNBR)
Overview of materials for Ethylene Vinyl Acetate Copolymer (EVA), Molded/Extruded
LyondellBasell Lucalen A2700M Low Density Polyethylene
ExxonMobil LDPE LD 202.48 Low Density Polyethylene Resin
Eastman 18DOA Polyethylene

PDIAM439 / 126530

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.