MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

(Viewing data as-entered. Click here to return)
Sika SilBridge-300 Elastomeric Silicone Profile
Categories: Polymer; Adhesive; Thermoset; Silicone; Silicone, RTV, Adhesive/Sealant Grade

Material Notes: Sika Silbridge-300 products are extruded ultra low modulus elastomeric silicone profiles that are usually bonded to substrates using Sikasil WS-295 sealant as an adhesive. Sika Silbridge-300 comes in a variety of standard shapes, colors and sizes and is successfully used in various applications.

Where to Use: Sika Silbridge-300 extruded profiles are specifically designed for numerous applications including but not limited to:

  • Expansion joint seals (new & remedial construction)
  • Window perimeter joint seals
  • Roofing Seals
  • Fillet beads, coping joints and window seals (custom design)
  • EIFS systems renovation
  • Metal Curtain Wall
Advantages:
  • High tear resistance
  • Ease of installation
  • Color fast formulation
  • Wide operational temperature range
  • Non corrosive and corrosion resistant
  • Resistant to ultraviolet exposure and weathering
  • Capable of sealing high movement joints
  • Reduces stress at bond-line making it well suited for soft and sensitive substrates such as EIFS
  • Rapid cure of thin adhesive layer allows for early movement of substrates
  • Economical alternative to cutting out existing failed sealant
Colors include White, Black, Limestone, Aluminum Gray, Colonial White, Bronze, and Medium Bronze, plus custom.

Information provided by Sika Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 20 - 30ASTM D2240
Tensile Strength 425 psiASTM D412
Elongation at Break 950 %ASTM D412
Tear Strength 70.0 pliDie B; ASTM D624
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 300 °F
Minimum Service Temperature, Air -60.0 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSIKA916 / 209823

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.