MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Ovako 34CrNiMo6 356D Steel, +SA
Categories: Metal; Ferrous Metal; Alloy Steel; AISI 4000 Series Steel

Material Notes: General Information: 34CrNiMo6 is a quenching and tempering steel with high strength, high toughness and good hardenability. Used for large axles, machine components, tools and high strength fasteners. The steel can be induction hardened and it is weldable under certain conditions. Through hardenability to appr. 100 mm diameter bar with oil quenching.
356D - Standard steel variant
356Q - IQ (isotropic quality) variant.
6499 - low sulphur variant of 34CrNiMo6
6507 - M-steel variant of 34CrNiMo6

IQ-SteelIQ-Steel® is an isotropic quality ultra clean steel optimized for high fatigue strength under multi axial loading.

Information provided by Ovako

Key Words: 34CrNiMo6M, 356, 356D, SS2541, MoCN315, MoCN315M, 1.6582, 35NCD6, 816M40, 817M40, 35NiCrMo6, SNCM447, 30Ch2N2MA, F.1272, 40NiCrMo7, 4337, 4340, 92541, VSQT34CrNiMo6, VSQT34CrNiMo6/700, VSQT34CrNiMo6/800, VSQT34CrNiMo6/900, Stål 2541, Steel 2541, EN24
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 7.80 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 200
@Thickness <=190 mm
Round bar
Modulus of Elasticity 210 GPa
Poissons Ratio 0.30
Shear Modulus 80.0 GPa
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.00000200 - 0.00000250 ohm-cm
 
Thermal PropertiesOriginal ValueComments
CTE, linear 12.0 µm/m-°C
@Temperature 20.0 - 300 °C
Specific Heat Capacity 0.460 - 0.480 J/g-°C
@Temperature 50.0 - 100 °C
Thermal Conductivity 40.0 - 45.0 W/m-KAmbient temperature
Transformation Temperature 315 °CMS
 725 °CAC1
 785 °CAC3
 
Component Elements PropertiesOriginal ValueComments
Carbon, C 0.32 - 0.38 %
Chromium, Cr 1.35 - 1.6 %
Iron, Fe 94.87 - 95.91 %As Balance
Manganese, Mn 0.70 - 0.80 %
Molybdenum, Mo 0.20 - 0.25 %
Nickel, Ni 1.3 - 1.6 %
Phosphorus, P <= 0.025 %
Silicon, Si 0.20 - 0.35 %
Sulfur, S 0.020 - 0.030 %
Vanadium, V <= 0.10 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Ovako 34CrNiMo6 356D Steel, +QT
Ovako 34CrNiMo6 356D Steel, Hardening
Ovako 34CrNiMo6 356Q Steel, Hardening
Ovako 34CrNiMo6 6499 Steel, +QT
Ovako 34CrNiMo6 6499 Steel, Hot forging

NOVAKO251 / 234550

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.