MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Extreme Materials from MCAM
Visit Mitsubishi Chemical Advanced Materials for Extreme Materials - high performance plastic machining stock engineered to replace metals such as nickel alloys or stainless steel.

(Viewing data as-entered. Click here to return)
Sandvik Kanthal SW 806 Spray Wire
Categories: Metal; Nonferrous Metal; Nickel Alloy

Material Notes: KANTHAL SW 806 is an austenitic NiAl alloy wire developed for use in Arc and Flame Spray systems. The wire produces dense, well bonding coatings. Typical applications are as bond coats, as protective coatings against high temperature oxidation, protective coatings against scaling of conventional iron base alloys, and as build up coatings for dimensional restoration.

Information provided by Sandvik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 8.20 g/cc
Porosity 3.0 - 7.0 %
 
Mechanical PropertiesOriginal ValueComments
Hardness, Vickers 180 - 250300g
Tensile Strength, Ultimate 850 MPa
Tensile Strength, Yield 780 MPa
@Strain 0.2 %
Elongation at Break 7.0 %
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000420 ohm-cm
@Temperature 20.0 °C
 
Thermal PropertiesOriginal ValueComments
Melting Point 1430 °C
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al >= 4.5 %
Nickel, Ni <= 95.5 %
 
Descriptive Properties
Deposition efficiency, %60-70
Oxides, %10-25
Surface Roughness, microns15-28

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

NSANDV262 / 19156

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.