MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Wacker Silres® BS 4004 Silicone Masonry Water Repellent
Categories: Polymer; Thermoset; Silicone

Material Notes: SILRES® BS 4004 is a water-thinnable, solventless emulsion, based on a mixture of silane and siloxane. Dilute solutions of SILRES® BS 4004 serve as high quality, general-purpose water repellents for hydrophobic impregnating and priming mineral surfaces. Mineral substrates treated with SILRES® BS 4004 are especially characterized by an excellent beading effect. Moreover SILRES® BS 4004 can be used for the mass hydrophobation of non-load bearing concrete products.

Properties: SILRES® BS 4004 emulsion contains a stabilized mixture of silanes and siloxanes that are susceptible to hydrolysis. Hydrolysis occurs only after application tothe substrate, which breaks the emulsion. Alcohol is released and the emulsion is converted into a silicone resin water repellent. SILRES® BS 4004 reduces the capillary absorption of the building which it has penetrated, but does not clog pores or capillaries. There is therefore little or no impairment of the building material´s ability to "breathe".

Special features:

  • good depth of penetration
  • rapid development of water repellency
  • highly durable and effective beading effect
  • tack-free drying
  • provides good adhesion for paints
  • water-based and environmentally compatible
  • stable in storage, even when diluted
Application: Dilute SILRES® BS 4004 is an excellent water repellent for many absorbent mineral substrates, such as bricks, sand-lime brick, natural sandstone and mineral plasters. It is not so suitable for less absorbent, dense natural stone, especially limestone, marble and reinforced concrete for bridges and roads. Owing to its aqueous consistency and storage stability when diluted, SILRES® BS 4004 is ideal for inplant impregnation of building materials made of clay, aerated concrete, sand-lime brick, fibrous cement, mineral fibers and lightweight aggregate. SILRES® BS 4004 may also serve as a water-repellent primer for emulsion paints and plasters, silicone resin emulsion paints and silicone resin plasters.

Information provided by Wacker Chemie AG.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.950 g/cc
Viscosity 12 cPdynamic
 
Descriptive Properties
Active ingredients (%)50
Appearancemilky, white

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PWACK9557 / 205086

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.