Telcar TL-2934N is a high performance UL V-0 flame retardant thermoplastic elastomer designed for electrical applications requiring flexibility over a wide temperature range. It is a high hardness, high density, low flow grade that is UV stabilized and RoHS compliant. This UL listed grade is easily colorable and is suitable for injection molding and extrusion. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North America Features: Brominated; Filled; Flame Retardant; General Purpose; Good Colorability; Halogenated; High Density; High Elongation; High Hardness; Low Flow; High Specific Gravity; High Tensile Strength; Sunlight Resistant (720 hrs); UV Resistant Uses: Appliance Wire Insulation; Appliance Wire Jacketing; Cable Jacketing; Connectors; Flexible Cord Jacketing; Industrial Cable Insulation; Ribbons; Rubber Replacement; Terminal Cable Jacketing; Underground Power Cable; Wire & Cable Applications; Wire Jacketing RoHS Compliant:RoHS UL File Number: QMFZ2.E54709 Form: Pellets Processing Method: Injection Molding; Extrusion Information provided by Teknor Apex |