MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Kostat ICP-STAT ICS-1004 PVC Sheet
Categories: Polymer; Thermoplastic; Vinyl (PVC)

Material Notes: KOSTATs ICP-STAT is a thermoplastic sheet coated with an inherently conductive polymer (ICP). ICP-STAT has distinctive advantages in ESD and cleanliness performances compared to other materials based on Hygroscopic Antistats and Conductive Fillers. This product exhibits superior transparency and clarity.

Special Features:

  • Superior Permanent Static Dissipation
  • Humidity Insensitivity
  • Excellent Wear resistance
  • Low Particle Generation
  • Superior Transparency and Clarity
  • Low Ionic Contamination
  • Excellent Chemical Resistance with Environmentally Friendly Materials

Applications:

  • Semiconductors Packaging
  • LCD Components Packaging
  • HDD Components Packaging
  • Electrical & Electronics Packaging
  • Medical Devices Packaging
  • Clean Room Accessories

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.34 g/ccASTM D792
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 6700 psiASTM D638
 
Electrical PropertiesOriginal ValueComments
Surface Resistivity per Square 1e+05 - 1.00e+6 ohmASTM D257
 1.00e+6 ohmafter 100% elongation; ASTM D257
 1.00e+7 ohmafter 200% elongation; ASTM D257
 1.00e+9 ohmafter 250% elongation; ASTM D257
 
Optical PropertiesOriginal ValueComments
Transmission, Visible >= 90 %ASTM D1003

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for PVC, Sheet Grade
GeonĀ® Performance Solutions 87725 Sheet PVC
Spartech SP-3010 Rigid PVC Specialty Sheet
GeonĀ® Performance Solutions 87655 Sheet PVC
Kostat ICP-STAT ICD-1004 PVC Sheet

PKOSTAT12 / 49047

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.