Product description: Grilon TSS/4 LF 2 is a heat stabilized, normal viscosity PA66 + PA6 injection molding grade with 2% lubricant (molybdenum disulphide). Grilon TSS/4 LF 2 has the following important properties:- Low sliding friction
- High surface hardness
- Short cycle times
Grilon TSS/4 LF 2 is typically used for oil dip sticks, low stressed slide rings, and damping elements.Information provided by EMS Grivory. |