System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
(Viewing data as-entered.
Click here
to return)
Teknor Apex Chemlon® 240 MH Nylon 6, 40% Short Glass Fiber Reinforced
Categories:
Polymer
;
Thermoplastic
;
Nylon (Polyamide PA)
;
Nylon 6 (PA6)
;
Nylon 6, 40% Glass Fiber Filled
;
Nylon 6, Glass Fiber Filled, Flame Retardant
Material Notes:
Features:
Heat Stabilized; Warp Resistant
Forms:
Pellets
Additive:
Heat Stabilizer
Automotive Specifications:
GM GMP.PA6.011
Information Provided by Teknor Apex
Key Words:
Polyamide 6
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Specific Gravity
1.51
g/cc
ASTM D792
Linear Mold Shrinkage
0.0060
-
0.010
in/in
ASTM D955
Mechanical Properties
Original Value
Comments
Tensile Strength
13000
psi
ASTM D638
Elongation at Break
4.0 %
ASTM D638
Elongation at Yield
3.9 %
ASTM D638
Flexural Strength
20800
psi
ASTM D790
Flexural Modulus
850000
psi
ASTM D790
Izod Impact, Notched
1.10
ft-lb/in
@Temperature 22.8 °C
ASTM D256
Electrical Properties
Original Value
Comments
Volume Resistivity
1.00e+14
ohm-cm
ASTM D257
Dielectric Strength
280
V/mil
@Thickness 3.00 mm
ASTM D149
Comparative Tracking Index
500
V
UL 746
Thermal Properties
Original Value
Comments
CTE, linear
31.0
µin/in-°F
ASTM D696
Deflection Temperature at 1.8 MPa (264 psi)
300
°F
Unannealed; ASTM D648
Flammability, UL94
HB
@Thickness 0.810 mm
Oxygen Index
23 %
ASTM D2863
Processing Properties
Original Value
Comments
Rear Barrel Temperature
425
-
455
°F
Middle Barrel Temperature
485
-
495
°F
Front Barrel Temperature
485
-
515
°F
Nozzle Temperature
485
-
515
°F
Melt Temperature
420
°F
480
-
515
°F
Processing Temperature
Drying Temperature
175
°F
Moisture Content
0.20 %
Descriptive Properties
Suggested Regrind, max
25
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
Users viewing this material also viewed the following:
Teknor Apex Chemlon 240 G Nylon 6, 43% Glass Fiber Reinforced
RTP Company RTP 207E TFE 10 Amorphous Nylon (Am. PA) Glass Fiber 40% - PTFE 10%
RTP Company RTP 207E Amorphous Nylon (Am. PA) Glass Fiber 40%
Omni Plastics OmniLon™ PA6 U GR43 BK1000 Nylon 6, 43% Glass reinforced
Domo TECHNYL® 2412GHF8 PA66, 40% glass fiber, DRY
PTEKNO412 / 128589
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.