Notes: Sarlink EE-2275N is a general purpose thermoplastic elastomer designed for automotive exterior applications. Sarlink EE-2275N exhibits good elastic properties with sunlight resistance and UV absorbing characteristics. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North America Features: Filled; High Density; Low Flow; High Specific Gravity; Light Stabilized; Medium Hardness; Sunlight Resistant; UV Absorbing Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim RoHS Compliance: RoHS Compliant Form: Pellets Processing Method: Extrusion Information provided by Teknor Apex |