MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Honeywell ACCUGLASS® T11 311 Spin-on Glass
Categories: Ceramic; Glass

Material Notes: The Accuglass T-11 (k = 3.8) Spin-on Glass (SOG) Series is a family of methylsiloxane polymers used for interlevel and overcoat passivation in the manufacture of integrated circuits. The AccuglassT-11 series is specially formulated to fill narrow (down to 0.3µm), high aspect ratio (up to 4) gaps without voids while planarizing multi-level metal devices. AccuglassT-11 contains 10 wt% CH3 (methyl) groups bonded to Si atoms in the Si-O backbone. The specific formulation results in a stable dielectric constant, high crack resistance, excellent gap fill and planarization properties of the cured film. Thin films of AccuglassT-11 are applied using a commercial coater and cured in a vertical or horizontal furnace to thicknesses up to 3800Å (single coat) and 6000Å (double coat).

Benefits

  • Industry proven performance and broad acceptance
  • T-11 fills gaps as small as 0.3µm
  • High thermal stability. Compatible with hot aluminum and tungsten plug processing. Permeability allows for hydrogen annealing of gate oxides
  • Thickness variation within a wafer of less than 1%. Wafer to wafer variation of less than 2%
  • Lower dielectric constant compared to silicates and phosphorus silicates
  • Crack resistance up to 6000Å
  • Good adhesion to top and bottom dielectric layers
Applications:
  • ILD and PMD Planarization
  • Overcoat Passivation
  • Gapfill
AccuglassT-11 is suitable for gap fill and planarization of ILD and PMD structures used in multilevel metal IC devices. Typically, partial etchback (PEB) is used for ILD and total etchback (TEB) is used for PMD. AccuglassT-11 can also be used to improve planarization of the final passivation layer.

Information provided by Honeywell

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Tensile Stress 120 MPa
 
Electrical PropertiesOriginal ValueComments
Dielectric Constant 3.8
@Frequency 1e+6 Hz
 
Thermal PropertiesOriginal ValueComments
CTE, linear 5.00 µm/m-°C
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.39
@Wavelength 633 nm
 
Processing PropertiesOriginal ValueComments
Shelf Life 1.25 Month
@Temperature 23.0 °C
 6.00 Month
@Temperature 4.00 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Honeywell ACCUGLASS® T11 111 Spin-on Glass
Honeywell ACCUGLASS® T12B 512B Spin-on Glass
Honeywell ACCUGLASS® P-5S Spin-on Glass
Honeywell ACCUGLASS® T11 211 Spin-on Glass
Honeywell ACCUGLASS® T12B 412B Spin-on Glass

PHONWL078 / 179623

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.