MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
NAECO® NAECOMET® 3950 AMS-T-21014 ASTM B777 High Density Machinable Tungsten
Categories: Metal; Nonferrous Metal; Refractory Metal; Tungsten Alloy

Material Notes: Uses: Radiation Shielding, High Mass, Gyro, Ordnance. Machinability is similar to gray iron.

Information provided by NAECO, LLC.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 18.0 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell A 63
@Temperature 600 °C
40 HRA
Hardness, Rockwell C 28
Tensile Strength, Ultimate 896 MPa
Tensile Strength, Yield 621 MPa
Elongation at Break 15 %
Modulus of Elasticity 365 GPa
Compressive Yield Strength 621 MPa
Fatigue Strength 465 MPaHigh cycle unnotched
 465 MPaHigh cycle unnotched
Charpy Impact 4.70 JNotched
Charpy Impact, Unnotched 54.2 J
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000133 ohm-cm
 
Thermal PropertiesOriginal ValueComments
CTE, linear 4.60 µm/m-°C
@Temperature 20.0 - 400 °C
 5.80 µm/m-°C
@Temperature 20.0 - 800 °C
Thermal Conductivity 110 W/m-K
Melting Point 1425 - 3410 °C
Solidus 1425 °C
Liquidus 3410 °C
 
Component Elements PropertiesOriginal ValueComments
Iron, Fe 1.5 %
Nickel, Ni 3.5 %
Tungsten, W 95 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
NAECO® NAECOMET® 2000 AMS-T-21014 ASTM B777 High Density Machinable Tungsten
NAECO® NAECOMET® 1000 AMS-T-21014 AMS-7725 ASTM B777 High Density Machinable Tungsten
Milliken® VelaCarb 335 Carbon Fiber Fabric
NAECO® NAECOMET® 2925 AMS-T-21014 ASTM B777 High Density Machinable Tungsten
NAECO® NAECOMET® 3970 AMS-T-21014 ASTM B777 High Density Machinable Tungsten

NCMV806 / 192357

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.