MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Kennametal Stellite Deloro® 716 PM cast
Categories: Metal; Nonferrous Metal; Nickel Alloy; Superalloy

Material Notes: Adhesive wear test data: cast 0.1; abrasive wear test data: cast 63 mm^3. Typical applications include vane plugs, fuel metering pins, spacer bushings, ball bearing blanks, race bearing blanks, diesel engine exhaust, fluid valve seats, saw cutter inserts, miscellaneous wear parts. Data provided by the manufacturer, Deloro Stellite Inc.

Product of former Deloro Stellite Inc.

Vendors: Visit metalmen for your metals needs. Products include special chemistry, tight tolerances, custom tempers, odd dimensions/forms, and small quantities. Phone 1-800-767-9494.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 8.17 g/cctheoretical
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 298Converted from Rockwell C hardness.
 154
@Temperature 760 °C
Converted from Rockwell B hardness
 228
@Temperature 649 °C
Converted from Rockwell C hardness
 259
@Temperature 538 °C
Converted from Rockwell C hardness
Hardness, Knoop 354Converted from Rockwell C hardness.
 180
@Temperature 760 °C
Converted from Rockwell B hardness
 268
@Temperature 649 °C
Converted from Rockwell C hardness
 306
@Temperature 538 °C
Converted from Rockwell C hardness
Hardness, Rockwell A 66Converted from Rockwell C hardness.
 50
@Temperature 760 °C
Converted from Rockwell C hardness
 60
@Temperature 649 °C
Converted from Rockwell C hardness
 63
@Temperature 538 °C
Converted from Rockwell C hardness
Hardness, Rockwell B 106Converted from Rockwell C hardness. Beyond normal Rockwell B scale, for comparison only.
 87
@Temperature 760 °C
Hardness, Rockwell C 32
 20
@Temperature 649 °C
Hot hardness.
 26
@Temperature 538 °C
Hot hardness.
Hardness, Vickers 309Converted from Rockwell C hardness.
 156
@Temperature 760 °C
Converted from Rockwell B hardness
 234
@Temperature 649 °C
Converted from Rockwell C hardness
 267
@Temperature 538 °C
Converted from Rockwell C hardness
 
Component Elements PropertiesOriginal ValueComments
Boron, B 0.40 %
Carbon, C 1.1 %
Chromium, Cr 26 %
Cobalt, Co 12 %
Iron, Fe 29 %
Molybdenum, Mo 3.0 %
Nickel, Ni 23 %As Remainder
Tungsten, W 3.5 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Kennametal Stellite Deloro® 711 PM cast
Kennametal Stellite Deloro® 208 PM cast
Kennametal Stellite Deloro® N-6 PM cast
Kennametal Stellite Stellite® 25 Cobalt Chromium Cast Alloy
Kennametal Stellite Deloro® 40G

ND716B / 16088

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.