MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
3M Scotch-Weld™ DP190 Gray Epoxy Adhesive
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: 3M™ Scotch-Weld™ Epoxy Adhesive DP190 Gray is a 1:1 mix ratio similar to Scotch-Weld™ Epoxy Adhesive 2216 B/A Gray and exhibits good peel, shear and environmental aging properties.

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Brookfield Viscosity 40000 - 80000 cPAccelerator, RFV #7 at 20 rpm
 75000 - 150000 cPBase, RFV #7 at 20 rpm
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 60ASTM D2240
Tensile Strength at Break 24.1 MPaASTM D882
Elongation at Break 30 %ASTM D882
Shear Strength 50.0 psiOverlap, Polypropylene
 300 psiOverlap, Glass, Borosilicate
 300 psiOverlap, Glass, +3M Scotch-Weld Primer 3901
 500 psiOverlap, Acrylic
 700 psiOverlap, ABS
 800 psiOverlap, Polycarbonate
 800 psiOverlap, PVC
 1100 psiOverlap, Wood, Fir
 1400 psiOverlap, CRS
 1500 psiOverlap, Sanded Aluminum
 1600 psiOverlap, Fiberglass
 2500 psiOverlap, Etched Aluminum
 400 psi
@Temperature 82.0 °C
Overlap
 600 psi
@Temperature 66.0 °C
Overlap
 1000 psi
@Temperature 49.0 °C
Overlap
 1500 psi
@Temperature -55.0 °C
Overlap
 2500 psi
@Temperature 21.0 °C
Overlap
Peel Strength 2.00 pli
@Temperature 82.0 °C
180°
 3.00 pli
@Temperature -55.0 °C
180°
 4.00 pli
@Temperature 66.0 °C
180°
 10.0 pli
@Temperature 49.0 °C
180°
 20.0 pli
@Temperature 21.0 °C
180°
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 5.00e+12 ohm-cmASTM D257
Dielectric Constant 6.5
@Frequency 1000 Hz
ASTM D150
Dielectric Strength 830 kV/in
@Thickness 0.762 mm
ASTM D149
Dissipation Factor 0.090
@Frequency 1000 Hz
ASTM D150
 
Thermal PropertiesOriginal ValueComments
CTE, linear 62.0 µm/m-°C
@Temperature 5.00 - 25.0 °C
Below Tg
 177 µm/m-°C
@Temperature 65.0 - 140 °C
Above Tg
Thermal Conductivity 0.381 W/m-K
@Thickness 6.35 mm,
Temperature 43.3 °C
Glass Transition Temp, Tg 7.00 °COnset
 20.0 °CMid-Point
 
Processing PropertiesOriginal ValueComments
Cure Time 8.00 - 12.0 hourTime to Handling Strength
 168 hourFull Cure
Tack-Free Time 6.00 hour
 
Descriptive Properties
AppearanceGrayAccelerator
 Gray
 WhiteBase

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
3M Scotch-Weld™ DP125 Gray Epoxy Adhesive
3M Scotch-Weld™ DP620NS Structural Adhesive
3M Scotch-Weld™ DP420 Black Epoxy Adhesive
Momentive Performance Materials RTV566 Red Extreme High Temperature Potting/Encapsulating Compound
Saint-Gobain Vitreosil® CFQ/TSC Optical Fused Quartz

PMM34651 / 169398

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.