MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

(Viewing data as-entered. Click here to return)
Master Bond MasterSil 930 Silicone
Categories: Polymer; Adhesive; Thermoset; Silicone

Material Notes: Key Features:
  • Paste consistency
  • Longer open time
  • Good physical strength profile
  • Superior chemical resistance
Product Description: MasterSil 930 is an acetoxy type fluorosilicone for bonding, sealing and coating. Its most prominent feature is enhanced chemical resistance, particularly to fuels, oils and solvents when compared to more standard silicones. Some of the chemicals that this product can withstand better than conventional silicones include gasoline, diesel fuel, motor oil and ethanol, among others. This system is an excellent adhesive that bonds well to a wide variety of substrates including metals, composites, ceramics, glass as well as many rubbers and plastics. MasterSil 930 can withstand the most aggressive types of thermal cycling as well as mechanical and thermal shock. Typical of one part silicones, the curing mechanism is based on the humidity level. The higher it is, the faster the cure and thinner sections cure more quickly than thicker ones. MasterSil 930 is a relatively fast curing system, and depending upon the application, the tack free time can range from 20-30 minutes. The full cure is typically recommended to be 3-4 days at ambient temperatures and humidity. As mentioned previously, it is noteworthy for is chemical resistance properties. Included in this list are water, many oils, fuels, greases, refrigerants, along with some acids and bases. Its service temperature range is -85°F to +450°F. It is important to note that MasterSil 930 has good adhesion to silicone substrates. MasterSil 930 is useful in a number of applications in aerospace, electronics, specialty OEM and other industries where the combination of flexibility, temperature resistance and chemical resistance is required

Information provided by Master Bond Inc.

Vendors: Master Bond is a leading manufacturer of adhesives, sealants, coatings and potting compounds. Master Bond’s vast product line consists of over 3,000 epoxy, polyurethane, silicone, cyanoacrylate and latex adhesives that vary in viscosity, cure speed, strength, chemical resistance, electrical properties, etc. Our custom adhesives offer design flexibility and provide excellent bonding performance. Visit www.masterbond.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.40 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 30 - 40
Tensile Strength 800 - 1100 psi
Elongation at Break 300 - 500 %
Adhesive Bond Strength 300 - 400 psiTensile Lap, Aluminum to Aluminum
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+14 ohm-cm
Dielectric Constant 6.08
@Frequency 60 Hz
Dissipation Factor 0.0030
@Frequency 60 Hz
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 450 °F
Minimum Service Temperature, Air -85.0 °F
 
Processing PropertiesOriginal ValueComments
Tack-Free Time 20.0 - 30.0 min
Shelf Life 6.00 Monthin original, unopened containers
 
Descriptive Properties
Chemical ResistanceAcetoneFair
 Brake fluidExcellent
 Crude oilGood
 Diesel fuelFair
 EthanolFair to good
 Ethylene glycolGood
 GasoholFair
 GasolineGood
 Isopropyl alcoholGood
 JP4 jet fuelGood to excellent
 Mineral oilExcellent
 Potassium hydroxide 25%Excellent
 SAE no. 20 oilGood
 Skydrol 500BExcellent
 Sodium hydroxide 25%Good
 SteamNot recommended
 Sulfuric acid 30%Good
 TolueneNot recommended
 WaterExcellent
 XyleneNot recommended
Colorwhite
Viscositypaste

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Dow Silastic® LS 4-9080 FLUOROSILICONE RUBBER
Dow Silastic® LS 4-9062 FLUOROSILICONE RUBBER
Dow Silastic® LS 4-9060 FLUOROSILICONE RUBBER
Dow Silastic® LS 4-9040 FLUOROSILICONE RUBBER
Dow Silastic® LS 4-9038 FLUOROSILICONE RUBBER

PMASTM943 / 185536

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.