MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
LyondellBasell Petrothene GA568200 Linear Low Density Polyethylene (LLDPE), Injection Molded
Categories: Polymer; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE); Linear Low Density Polyethylene (LLDPE), Injection Molded

Material Notes: Petrothene GA568200 exhibits an excellent balance of processability, stiffness, impact strength and ESCR. Typical applications include house wares, trash cans, medical items and closures. Applications: House wares, Industrial Packaging, Outdoor and Power Tools, Sports, Leisure & Toys, Trash Cans

Information provided by LyondellBasell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.925 g/ccASTM D1505
Melt Flow 33 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
Spiral Flow 40.1 cmLYB Method
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 58ASTM D2240
Tensile Strength at Break 8.00 MPaASTM D638
Tensile Strength, Yield 14.0 MPaASTM D638
Elongation at Yield 12 %ASTM D638
Flexural Modulus, 1% Secant 460 MPaASTM D790
2% Secant Modulus 390 MPaASTM D790
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 46.0 °Cunannealed; ASTM D648
Vicat Softening Point 87.0 °CASTM D1525
Brittleness Temperature <= -76.0 °CASTM D746
 
Descriptive Properties
Processing MethodInjection Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
LyondellBasell Petrothene GA574200 Linear Low Density Polyethylene (LLDPE), Injection Molded
LyondellBasell Petrothene GA578189 Linear Low Density Polyethylene (LLDPE), Injection Molded
LyondellBasell Petrothene GA623119 Linear Low Density Polyethylene (LLDPE)/Hexene, Molded
Dow DOWLEX™ NG 2085 Linear Low Density Polyethylene, Ethylene-Octene Copolymer
Dow DOWLEX™ 2267G Linear Low Density Polyethylene

PEQT8822 / 220456

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.