MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
NanoScale NanoActive® Magnesium Oxide  (discontinued **)
Categories: Ceramic; Oxide; Magnesium Oxide

Material Notes: NanoActive MgO is produced using proprietary processes to obtain high specific surface area, small crystallite size material possessing high chemical reactivity, particularly at elevated temperatures.

Applications: Applications include destruction of chemical warfare agents, destructive adsorption of acid gases and polar organic molecules, fertilizers, nanocomposites, phosphor particle protection layer, precursor for other magnesium chemicals, remediation of toxic waste, sintering aid, and waste water treatment.

Information provided by NanoScale

Composition based on metal

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 0.600 g/cc
Density 3.20 g/cc
Moisture Absorption <= 1.0 %
Loss On Ignition <= 8.0 %
Particle Size 3.3 µmmean aggregate size
Specific Surface Area >= 230 m²/gBET
Pore Size 0.00500 micronsAverage Diameter
 
Component Elements PropertiesOriginal ValueComments
Magnesium, Mg >= 95 %
 
Descriptive Properties
Appearance / ColorWhite Powder
Crystallite Size= 8 nm
Minimum Total Pore Volume cc/g0.2

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
CeramTec Sikor® S Cordierite
Morgan Advanced Ceramics Luminex™ 993 Magnesia
Aremco Ceramacast™ 672 High Temperature Potting & Casting Material Magnesia
MarkeTech Repton EXP 22 Magnesia MgO
MarkeTech Repton 914 Magnesia MgO

CNANO05 / 1667

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.