MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Total Lumicene® mPE M 2710 EP Metallocene Polyethylene, Blown Film
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE); Linear Low Density Polyethylene (LLDPE), Film Grade; LLDPE/Hexene, Film Grade

Material Notes: Lumicene® mPE M 2710 EP is a second generation metallocene based Low Density Polyethylene with hexene as comonomer.

Lumicene® mPE M 2710 EP can be processed at high output rates with low extrusion pressure, excellent bubble stability and gauge control in comparison with conventional LLDPE and first generation metallocene based polyethylene. The combination of these features brings a significant downgauging potential.

Lumicene® mPE M 2710 EP is especially dedicated to film applications where high gloss and high transparency are required, particularly in blend and coextrusion with LLDPE or LDPE.

Lumicene® mPE M 2710 EP is suited for many applications in the field of consumer, industrial, food or hygiene packaging such as bags, deep freeze, collation shrink and lamination.

Information provided by Total Petrochemicals. Also available in the Americas from the Bayport Polymers joint venture.

Key Words: High output rates with low extrusion pressure
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.927 g/ccISO 1183
Thickness 40.0 microns
Melt Flow 0.90 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Film Tensile Strength at Yield, MD 13.5 MPaISO 527-3
Film Tensile Strength at Yield, TD 14.0 MPaISO 527-3
Film Elongation at Break, MD 650 %ISO 527-3
Film Elongation at Break, TD 720 %ISO 527-3
Elmendorf Tear Strength, MD 6.10 g/micronISO 6383-2
Elmendorf Tear Strength, TD 16.3 g/micronISO 6383-2
Dart Drop Test 200 gISO 7765-1
Film Tensile Strength at Break, MD 51.0 MPaISO 527-3
Film Tensile Strength at Break, TD 48.0 MPaISO 527-3
 
Thermal PropertiesOriginal ValueComments
Melting Point 119 °CISO 11357
Vicat Softening Point 118 °CISO 306
 
Optical PropertiesOriginal ValueComments
Haze 6.5 %ISO 14782
Gloss 70 %at 45°; ASTM D2457
 
Processing PropertiesOriginal ValueComments
Processing Temperature 180 - 230 °CBlow Molding
Melt Temperature 200 °CExtrusion
Die Opening 0.0800 - 0.280 cm
Blow-up Ratio (BUR) 1.5 - 4.5

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Total Lumicene® mPE M6040 S01 Metallocene Polyethylene, Cast Film
Total Lumicene® mPE M 2704 EP S01 Metallocene Polyethylene, Blown Film
Baystar™ Lumicene® mPE M 3410 EP Metallocene Medium Density Polyethylene Film Resin
UBE UMERIT 500F Metallocene LLDPE
LyondellBasell Petrothene® L3035 Low Density Polyethylene, Film Extrusion Grade

PTOTAL772 / 130497

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.