MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
3M Scotch-Weld™ 4550 Industrial Adhesive
Categories: Polymer; Adhesive

Material Notes:

Features:

  • It is a sprayable, synthetic elastomer based adhesive for bonding many lightweight materials such as felt, cork, cardboard, and paper to metal and other substrates
  • Ideal for palletizing “all-plastic” shipping bags, Holds bags in place during storage and shipment. When unstacking, bags separate easily with no bag tear.
  • Fast tacking; ideal for low pressure spray with minimal misting and cobwebbing. Offers high coverage and long bonding rage.

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Solids Content 36 - 38 %
Brookfield Viscosity 100 - 4000 cPRVF #4 sp @ 20 rpm @ 27°C
 
Mechanical PropertiesOriginal ValueComments
Peel Strength 12.0 pli180°, Scott Tensile Tester
 
Thermal PropertiesOriginal ValueComments
Flash Point -29.0 °CTCC
 
Processing PropertiesOriginal ValueComments
Shelf Life 6.00 Month
 
Descriptive Properties
AppearanceTranslucent
BaseSBR

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PMM34107 / 168854

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.