MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Aaron Industries AVPE LLD 300-2 Virgin Polyethylene
Categories: Polymer; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE)

Material Notes: Melt flow index may be specified.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.930 - 0.945 g/cc0.930 - 0.945 g/ccASTM D792
Linear Mold Shrinkage 0.015 cm/cm0.015 in/inASTM D955
Melt Flow 2.0 - 120 g/10 min
@Load 5.00 kg,
Temperature 190 °C
2.0 - 120 g/10 min
@Load 11.0 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 20.7 MPa3000 psiASTM D638
Flexural Modulus 0.724 GPa105 ksiASTM D790
Izod Impact, Notched NBNBASTM D256

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Dow DOWLEX™ 2505 Linear Low Density Polyethylene, Narrow MW Distribution
Mitsui ADMER® NF498A PE Type Polyolefin
Overview of materials for Linear Low Density Polyethylene (LLDPE), Injection Molded
LyondellBasell Petrothene® GA694189 Linear Low Density Polyethylene, Injection Molding Grade
LyondellBasell Petrothene® GA594189 Linear Low Density Polyethylene, Injection Molding Grade

PRONAA972 / 135303

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.